摘要: 为了分析简易机场的合理道面结构, 依托陕西西安、湖南耒阳的室内外试验段, 利用直径30cm刚性承载板模拟机轮荷载圆, 使用反力架、千斤顶及疲劳试验机, 通过人工和机械定点重复加载模拟飞机通行, 研究了薄层沥青混凝土面层+水泥稳定细粒土基(垫)层道面结构在重复荷载作用下的疲劳特性。试验结果表明: 推荐道面结构早期承载能力较高, 在60d龄期内, 整体回弹模量为200~300MPa, 弯沉小于1mm; 此时道面可承受飞机荷载几万至十几万次的起降通行而不破坏, 并保持良好的使用性能; 推荐道面结构的疲劳特性可以满足简易机场的应急使用需求。Abstract: In order to analyze the reasonable pavement structure of field airfield, indoor and outdoor trial roads were built in Xi'an of Shaanxi Province and Leiyang of Hunan Province, load circle induced by aircraft wheel was simulated by using rigid bearing plate with 30 cm diameter, the experimental equipments such as reaction frame, hoisting jack and fatigue machine were used, the taxiing of aircraft at the same point of the pavement was simulated through manual and mechanical repeated loadings, the fatigue characteristic of the pavement with thin asphalt concrete surface and cement stabilized fine grained soil base(or subbase) was studied. Experiment result shows that the early carrying capacity of the recommended pavement structure is better, holistic elastic modulus is between 200~300 MPa, and its deflection is less than 1 mm in 60 days. The structure has good using performance, and will not be destroyed after ten thousands to hundred thousands times of takeoff and landing of airplane. The fatigue characteristic of the structure can meet the emergency requirement of field airfield.
-
表 1 土样参数
Table 1. Soil parameters
表 2 水泥土性能指标
Table 2. Performance indexes of cement stabilized soil
表 3 西安试验段道面整体回弹模量
Table 3. Holistic elastic modulus of pavement in Xi'an
表 4 耒阳试验段道面整体回弹模量
Table 4. Holistic elastic modulus of pavement in Leiyang
表 5 弯沉结果
Table 5. Deflection results
-
[1] TM5-822-14, soil stabilization for pavements[S]. [2] 彭高丰. 薄层沥青混凝土道面在简易机场中的应用研究[D]. 西安: 空军工程大学, 2005. [3] GJB1112A—2004, 军用机场场道工程施工及验收规范[S]. [4] JTJ034—2006, 公路路面基层施工技术规范[S]. [5] JTG F40—2004, 公路沥青路面施工技术规范[S]. [6] 李进军, 黄茂松, 王育德. 交通荷载作用下软土地基累积塑性变形分析[J]. 中国公路学报, 2006, 19(1): 1-5. https://www.cnki.com.cn/Article/CJFDTOTAL-ZGGL200601000.htmLI Jin-jun, HUANG Mao-song, WANG Yu-de. Analysis of cumulative plastic deformation of soft clay foundation under traffic loading[J]. China Journal of Highway and Transport, 2006, 19(1): 1-5. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-ZGGL200601000.htm [7] 史保华, 许巍, 齐勇, 等. 机场沥青道面管理与预防性维护对策[J]. 交通运输工程学报, 2008, 8(2): 74-79. http://transport.chd.edu.cn/article/id/200802016SHI Bao-hua, XU Wei, QI Yong, et al. Management and preventive maintenance countermeasures of airport asphalt pavement[J]. Journal of Traffic and Transportation Engi-neering, 2008, 8(2): 74-79. (in Chinese) http://transport.chd.edu.cn/article/id/200802016 [8] 姚玉玲, 任勇, 陈拴发. 沥青路面的预防性养护时机[J]. 长安大学学报: 自然科学版, 2006, 26(6): 34-38. https://www.cnki.com.cn/Article/CJFDTOTAL-XAGL200606007.htmYAO Yu-ling, REN Yong, CHEN Shuan-fa. Preventive maintenance ti ming of asphalt pavement[J]. Journal of Chang an University: Natural Science Edition, 2006, 26(6): 34-38. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-XAGL200606007.htm [9] 杜顺成, 戴经梁. 沥青混合料永久变形评价指标[J]. 中国公路学报, 2006, 19(5): 18-22. doi: 10.3321/j.issn:1001-7372.2006.05.004DU Shun-cheng, DAI Jing-liang. Permanent deformation evaluation index of asphalt mixture[J]. China Journal of Highway and Transport, 2006, 19(5): 18-22. (in Chinese) doi: 10.3321/j.issn:1001-7372.2006.05.004