中国轨道交通轮轨滚动接触疲劳研究进展

赵鑫 温泽峰 王衡禹 陶功权 金学松

赵鑫, 温泽峰, 王衡禹, 陶功权, 金学松. 中国轨道交通轮轨滚动接触疲劳研究进展[J]. 交通运输工程学报, 2021, 21(1): 1-35. doi: 10.19818/j.cnki.1671-1637.2021.01.001
引用本文: 赵鑫, 温泽峰, 王衡禹, 陶功权, 金学松. 中国轨道交通轮轨滚动接触疲劳研究进展[J]. 交通运输工程学报, 2021, 21(1): 1-35. doi: 10.19818/j.cnki.1671-1637.2021.01.001
ZHAO Xin, WEN Ze-feng, WANG Heng-yu, TAO Gong-quan, JIN Xue-song. Research progress on wheel/rail rolling contact fatigue of rail transit in China[J]. Journal of Traffic and Transportation Engineering, 2021, 21(1): 1-35. doi: 10.19818/j.cnki.1671-1637.2021.01.001
Citation: ZHAO Xin, WEN Ze-feng, WANG Heng-yu, TAO Gong-quan, JIN Xue-song. Research progress on wheel/rail rolling contact fatigue of rail transit in China[J]. Journal of Traffic and Transportation Engineering, 2021, 21(1): 1-35. doi: 10.19818/j.cnki.1671-1637.2021.01.001

中国轨道交通轮轨滚动接触疲劳研究进展

doi: 10.19818/j.cnki.1671-1637.2021.01.001
基金项目: 

国家自然科学基金项目 51675444

中国-拉美和加勒比国家共同体轨道交通联合实验室项目 KY201701001

牵引动力国家重点实验室自主课题 2019TPL_T17

详细信息
    作者简介:

    赵鑫(1981-),男,山东新泰人,西南交通大学副研究员,工学博士,从事轮轨关系研究

  • 中图分类号: U270.1

Research progress on wheel/rail rolling contact fatigue of rail transit in China

Funds: 

National Natural Science Foundation of China 51675444

Project of China- CELAC United Laboratory for Rail Transit KY201701001

Independent Subject of State Key Laboratory of Traction Power 2019TPL_T17

More Information
  • 摘要: 系统阐述了轮轨滚动接触疲劳损伤的分类、萌生机理、影响因素、引发后果及常用萌生预测模型等,总结了其复杂性的根源; 梳理了中国轨道交通系统近年来发生的各种轮轨滚动接触疲劳的相关研究成果,分别总结了高速铁路、普速铁路和地铁等系统轮轨滚动接触疲劳的基本特征、萌生机理及治理措施等; 展示了在局部和连续型滚动接触疲劳研究中,现场跟踪测试、现场试样失效分析、试验台试验、数值模拟及线路试验等研究方法的系统化应用及重要结果; 讨论了不同轨道交通系统滚动接触疲劳差异的根本原因及滚动接触疲劳各影响因素的相对重要性,并从现场治理和机理研究2个方面提出了展望。研究结果表明:高速动车组轮轨局部型滚动接触疲劳(月牙形裂纹)对运营安全的威胁可控,其重要源头之一是硌伤; 过大的接触应力和蠕滑率是引发轮轨连续型滚动接触疲劳的关键,其根本原因包括小半径曲线、轮轨失形、轮轨廓形与轨道曲线设计不合理、大坡度与起伏坡度、低黏着与增黏、频繁启停及轨道安装误差等,近10年来开始大量使用的大功率电力机车在复杂条件线路运行时,呈现的严重车轮滚动接触疲劳是上述影响因素综合作用的集中体现; 可行的滚动接触疲劳防治措施包括避免或及时修复严重硌伤、优化曲线段轮轨廓形匹配、优化轮轨镟修/打磨策略、加装或优化车轮研磨子、机车车辆定期调头运行、优化机车电气补偿与牵引制动控制、使用优质增黏砂、优化踏面制动和及时维护轨道与列车关键部件等,不同轮轨系统可根据其特点酌情选用; 从现场防治角度,应建立轮轨滚动接触疲劳的精确预测模型,并依此实现不同服役条件下的滚动接触疲劳无限和有限寿命设计及最佳轮轨维修策略制定; 从疲劳机理角度,应重点研究疲劳裂纹萌生的微观裂纹扩展机制和磨耗影响机制。

     

  • 图  1  萌生于接触表面(左)和次表层(右)的轮轨滚动接触疲劳

    Figure  1.  Wheel/rail rolling contact fatigue initiated on contact surface (left) and subsurface (right)

    图  2  连续型轮轨滚动接触疲劳

    Figure  2.  Continuous wheel/rail rolling contact fatigue

    图  3  中国轮轨系统发现的典型局部型滚动接触疲劳

    Figure  3.  Typical local rolling contact fatigue occurring in Chinese wheel-rail systems

    图  4  典型滚滑状态下法、切向轮轨接触应力分布

    Figure  4.  Distributions of normal and tangential contact stresses under typical rolling-sliding state

    图  5  施加法、切向接触应力时轨头纵向截面(通过接触斑中心)V-M等效应力分布

    Figure  5.  Distributions of V-M equivalent stresses in longitudinal section of rail head (passing contact patch center) under normal and tangential contact stresses

    图  6  钢轨内V-M等效应力沿深度的分布

    Figure  6.  Distributions of V-M equivalent stress of rail along depth

    图  7  不同磨耗率下的轮轨接触表面损伤形态

    Figure  7.  Wheel/rail contact surface damage states under different wear rates

    图  8  轮轨服役寿命主导损伤形式随磨耗率的变化

    Figure  8.  Variation of damage form dominated by wheel and rail service life with wear rate

    图  9  液体对滚动接触疲劳裂纹扩展的影响

    Figure  9.  Influence of liquid on propagation of rolling contact fatigue crack

    图  10  撒增黏砂后的车轮接触表面

    Figure  10.  Wheel contact surfaces after sanding for adhesion enhancement

    图  11  安定图

    Figure  11.  Shakedown map

    图  12  循环载荷作用下的4种材料响应

    Figure  12.  Four types of material responses under cyclic loading

    图  13  英国BS11(R220)钢轨损伤函数模型

    Figure  13.  Damage function developed for UK BS11 (R220) rail

    图  14  车轮硌伤在法向接触载荷作用下的变形及V-M等效应力分布

    Figure  14.  Deformation and V-M equivalent stress distributions at wheel indentations under normal contact load

    图  15  GPM-30滚动接触疲劳试验台

    Figure  15.  GPM-30 test rig for rolling contact fatigue

    图  16  试验盘在轮轨中的取材位置及尺寸

    Figure  16.  Positions and dimensions of test discs manufactured from wheel and rail

    图  17  丝锥顶尖冲击硌伤演化

    Figure  17.  Evolvement of indentations impacted by tap tips

    图  18  最高速度200 km·h-1动车组上第1类车轮连续型滚动接触疲劳(2014年)

    Figure  18.  Type 1 continuous rolling contact fatigue of wheel on EMUs running at top speed of 200 km·h-1 (2014)

    图  19  城际线路动车组上第1类车轮连续型滚动接触疲劳(2017年)

    Figure  19.  Type 1 continuous rolling contact fatigue of wheel on intercity EMUs (2017)

    图  20  动车组车厢通过曲线时低轨侧车轮滚动接触疲劳预测结果

    Figure  20.  Rolling contact fatigue prediction results of wheels on low rail side of EMU coach when passing through curve

    图  21  不同镟后里程动车组车厢通过曲线时2轴低轨侧车滚动接触轮疲劳预测结果

    Figure  21.  Rolling contact fatigue prediction results of wheel on low rail side of axle 2 when EMU coach with different running distances after repairing passing through curves

    图  22  城际动车组匀速通过不同半径曲线时车轮的损伤函数预测结果(1轴导向)

    Figure  22.  Prediction results of wheels by damage function when intercity EMU passing curves of different radii at constant speed (axle 1 leads)

    图  23  某城际动车组运行线路上的曲线高轨滚动接触疲劳(2019)

    Figure  23.  Rolling contact fatigue on high rail of curve on an intercity EMU line (2019)

    图  24  华北某机务段A的C型大功率电力机车车轮滚动接触疲劳(2016)

    Figure  24.  Wheel rolling contact fatigue on C-type high power electric locomotive in railway bureau A in North China

    图  25  西北某机务段B的D型大功率电力机车车轮滚动接触疲劳(2016)

    Figure  25.  Wheel rolling contact fatigue on D-type high power electric locomotive in railway bureau B in Northwest China

    图  26  机务段A的C型大功率电力机车使用的增黏砂

    Figure  26.  Sands for adhesion enhancement used for C-type high power electric locomotive in railway bureau A

    图  27  机务段B的D型大功率电力机车使用的增黏砂

    Figure  27.  Sands for adhesion enhancement used for D-type high power electric locomotive in railway bureau B

    图  28  机车通过不同半径平面右曲线时3轴左轮滚动接触疲劳的损伤函数预测结果

    Figure  28.  Rolling contact fatigue of left wheel of axle 3 predicted by damage function when locomotive passing through right curves of different radii

    图  29  机车通过不同坡度直线时1轴左轮滚动接触疲劳的损伤函数预测结果

    Figure  29.  Rolling contact fatigue of left wheel of axle 1 predicted by damage function when locomotive passing through straight line tracks with different slopes

    图  30  机车通过半径800 m右曲线和直线时3轴左轮滚动接触疲劳损伤函数预测结果随坡度变化

    Figure  30.  Variations of rolling contact fatigue of left wheel of axle 3 with slope predicted by damage function when locomotive running on right curve of 800 m radius and straight line track

    图  31  机车通过半径600 m右曲线不同坡度时滚动接触疲劳预测结果

    Figure  31.  Rolling contact fatigue prediction results when locomotive running on right curve of 600 m radius with different slopes

    图  32  干态直线下坡工况下损伤函数预测结果

    Figure  32.  Prediction results by damage function under dry and downhill straight line track condition

    图  33  湿态直线下坡工况下损伤函数预测结果

    Figure  33.  Prediction results by damage function under wet and straight line track condition

    图  34  直线下坡工况下D型机车各轴左轮法向力

    Figure  34.  Normal forces on left wheels of D-type locomotive under downhill straight line track condition

    图  35  成都车辆段25G客车滚动接触疲劳裂纹

    Figure  35.  Wheel rolling contact fatigue crack on 25G passenger train in Chengdu

    图  36  朔黄重载线500 m半径曲线高轨斜裂纹平均长度和深度变化

    Figure  36.  Variations of average length and depth of oblique crack in high rail on curve of 500 m radius on Shuohuang Heavy Haul Line

    图  37  广深线K14+600处曲线高轨斜裂纹

    Figure  37.  Oblique cracks on high rail of curve at K14+600 of Guangshen Line

    图  38  中国A型地铁列车第2类车轮滚动接触疲劳

    Figure  38.  Type 2 wheel rolling contact fatigue of on A-type metro trains in China

    图  39  地铁动车通过不同半径曲线时各车轮的损伤函数疲劳峰值

    Figure  39.  Peak values of damage function of various wheels when metro motor passing through curves with different radii

    图  40  某地铁线路300 m半径曲线高轨上细条状滚动接触疲劳(U75V材质)

    Figure  40.  Long-strip rolling contact fatigue on high rail of metro line with radius of 300 m (U75V rail material)

    图  41  闸瓦磨耗导致地铁车轮轮缘根部出现台阶

    Figure  41.  Stair close to root of metro wheel flange resulting from braking shoe wear

    图  42  某地铁线路上由异常车轮磨耗导致的道岔心轨滚动接触疲劳

    Figure  42.  Rolling contact fatigue on point rail of turnout of metro line resulting from abnormal worn wheels

    表  1  不同轮轨系统的关键参数及其滚动接触疲劳特点

    Table  1.   Key parameters of different wheel/rail systems and characteristics of corresponding rolling contact fatigue

    铁路类型 高速 普速 城市地铁
    干线 城际 机车 客运 货运
    机车车辆 最高速度/(km·h-1) 200~350 ≤200 120、160 80~100 80~100
    轴重/t 14~17 21~23 14 21~25 14~16
    轮径/mm 860、915、920 1 250 915 840 840
    车轮廓形 LMA、S1002CN、LMB10 JM3 LM LM、DIN5573
    车轮材质 ER8 ER8、ER9、Grade 3 CL60 CL60、ER8、ER9
    轨道 最小半径/m 3 500(250 km·h-1)、7 000(350 km·h-1) 约350 约250 约200
    钢轨材质 U71MnG U71MnG、U75VG U71Mn、U75V和U78CrV等的热轧或热处理
    轨型 CHN60、CHN60N
    滚动接触疲劳 特点 车轮发生严重局部疲劳,偶见轻微连续型疲劳 发生轻微至中度连续型疲劳 复杂条件线路上车轮多发第1~3类连续疲劳,3类为最 车轮发生轻微第1类连续疲劳,小半径曲线钢轨中度连续疲劳 重载曲线轨发生中度至严重连续疲劳 发生中度至严重连续型疲劳
    原因 异物硌伤、轮轨过度失形、曲轨廓形不合理、研磨子作用不合理等 牵引/制动频繁,小半径曲线,曲线设计不合理,轮轨失形等 小半径曲线、大坡度、低黏着、增黏砂、制动力集中、轴重转移及不合理电气补偿等 小半径曲线、大坡度或起伏坡道、轮轨廓形不匹配、低黏着、增黏砂等 牵引/制动频繁,小半径曲线,曲线设计不合理,轮缘过度润滑,踏面制动磨耗,轮轨失形等
    应对措施 清理异物,及时维修深硌伤,曲轨廓形优化,监控轮轨失形,优化研磨子作用等 调头运行,曲线钢轨廓形优化,监控轮轨失形等 避免仅运行于杂条件线路,使用优质增黏砂,优化电气补偿和牵引/制动控制等 钢轨预打磨,曲线钢轨廓形优化,监控轮轨失形,使用合适强度的材质等 调头运行、轮轨廓形优化,监控轮轨失形,踏面制动优化,使用合适强度的材质等
    下载: 导出CSV
  • [1] 金学松, 沈志云. 轮轨滚动接触疲劳问题研究的最新进展[J]. 铁道学报, 2001, 23(2): 92-108. doi: 10.3321/j.issn:1001-8360.2001.02.019

    JIN Xue-song, SHEN Zhi-yun. Rolling contact fatigue of wheel/rail and its advanced research progress[J]. Journal of the China Railway Society, 2001, 23(2): 92-108. (in Chinese) doi: 10.3321/j.issn:1001-8360.2001.02.019
    [2] CANNON D F, EDEL K O, GRASSIE S L, et al. Rail defects: an overview[J]. Fatigue and Fracture of Engineering Materials and Structures, 2003, 26(10): 865-886. doi: 10.1046/j.1460-2695.2003.00693.x
    [3] SMITH R A. Railway fatigue failures: an overview of a long standing problem[J]. Material Science and Engineering Technology, 2005, 36(11): 697-705. http://www.onacademic.com/detail/journal_1000033884877610_2c93.html
    [4] GRASSIE S L. Rolling contact fatigue on the British Railway System: treatment[J]. Wear, 2005, 258(7/8): 1310-1318. http://www.sciencedirect.com/science/article/pii/S0043164804002996
    [5] LI Zi-li, DOLLEVOET R, MOLODOVA M, et al. Squat growth—some observations and the validation of numerical predictions[J]. Wear, 2011, 271(1/2): 148-157. http://www.sciencedirect.com/science/article/pii/S0043164810003856
    [6] KARTTUNEN K, KABO E, EKBERG A. The influence of track geometry irregularities on rolling contact fatigue[J]. Wear, 2014, 314(1/2): 78-86. http://www.sciencedirect.com/science/article/pii/S0043164813005838
    [7] GROHMANN H D, HEMPELMANN K A, GROB-THEBING A. A new type of RCF, experimental investigations and theoretical modeling[J]. Wear, 2002, 253(1/2): 67-74. http://www.sciencedirect.com/science/article/pii/S0043164802000844
    [8] BOGDA AN' NSKI S. Quasi-static and dynamic liquid solid interaction in 3D squat-type cracks[J]. Wear, 2014, 314(1/2): 20-27. http://www.sciencedirect.com/science/article/pii/S004316481300567X
    [9] TUNNA J, SINCLAIR J, PEREZ J. A review of wheel wear and rolling contact fatigue[J]. Proceedings of the Institution of Mechanical Engineer, Part F: Journal of Rail and Rapid Transit, 2007, 221(2): 271-289. doi: 10.1243/0954409JRRT72
    [10] 金学松, 张继业, 温泽峰, 等. 轮轨滚动接触疲劳现象分析[J]. 机械强度, 2002, 24(2): 250-257. doi: 10.3321/j.issn:1001-9669.2002.02.023

    JIN Xue-song, ZHANG Ji-ye, WEN Ze-feng, et al. Overview of phenomena of rolling contact fatigue of wheel/rail[J]. Journal of Mechanical Strength, 2002, 24(2): 250-257. (in Chinese) doi: 10.3321/j.issn:1001-9669.2002.02.023
    [11] CANNON D F. An international cross reference of rail defects[R]. Paris: International Union of Railways, 2003.
    [12] EKBERG A, KABO E. Fatigue of railway wheels and rails under rolling contact and thermal loading—an overview[J]. Wear, 2005, 258(7): 1288-1300. http://www.sciencedirect.com/science/article/pii/S0043164804002972
    [13] ZHANG Guan-zhen, REN Rui-ming. Study on typical failure forms and causes of high-speed railway wheels[J]. Engineering Failure Analysis, 2019, 105(1): 1287-1295. http://www.sciencedirect.com/science/article/pii/S135063071830654X
    [14] CONG Tao, HAN Jian-min, HONG Youshi, et al. Shattered rim and shelling of high-speed railway wheels in the very-highcycle fatigue regime under rolling contact loading[J]. Engineering Failure Analysis, 2019, 97(1): 556-567. http://www.sciencedirect.com/science/article/pii/S1350630718312172
    [15] DEUCE R. Wheel tread damage—an elementary guide[R]. Netphen: Bombardier Transportation Gmbh, 2007.
    [16] MAGEL E. Rolling contact fatigue: a comprehensive review[R]. Washington DC: U.S. Department of Transportation, 2011.
    [17] EKBERG A, KABO E, KARTTUNEN K, et al. Identifying the root causes of damage on the wheels of heavy haul locomotives and its mitigation[J]. Proceedings of the Institution of Mechanical Engineer, Part F: Journal of Rail and Rapid Transit, 2014, 228(6): 663-672. doi: 10.1177/0954409714526165
    [18] ZHAO Xin, WEN Ze-feng, LIU De-gang, et al. Observations and monitoring of the rolling contact fatigue of Chinese high-speed wheels[C]//GAO Xiao-rong. Proceedings of the 18th International Wheelset Congress. New York: IEEE, 2016: 55-59.
    [19] DOLLEVOET R. Design of an anti-head check profile based on stress relief[D]. Tenschede: University of Twente, 2010.
    [20] FLETCHER D I, FRANKLIN F J, KAPOOR A. Rail surface fatigue and wear[M]//LEWIS R, OLOFSSON U. Wheel-Rail Interface Handbook. New York: CRC Press, 2009: 280-310.
    [21] INNOTRACK. D4.1.4 Rail degradation algorithm[R]. Berlin: Corus Rail and voestalpine Schienen, 2009.
    [22] ZHAO Xin. Dynamic wheel/rail rolling contact at singular defects with application to squats[D]. Delft: Delft University of Technology, 2012.
    [23] ZHAO Xin, AN Bo-yang, ZHAO Xiao-gang, et al. Local rolling contact fatigue and indentations on high-speed railway wheels: observations and numerical simulations[J]. International Journal of Fatigue, 2017, 103(1): 5-16. http://www.sciencedirect.com/science/article/pii/S0142112317302281
    [24] LUTHER M, MÄDLER K, HEYDER R. Prevention of multiple squats and rail maintenance measures[C]//LI Zi-li, NUNEZ A. Proceedings of the 11th International Conference on Contact Mechanics and Wear of Rail/Wheel Systems. Delft: Delft University of Technology, 2018: 618-622.
    [25] ZHAO Xin, WANG Zhe, WEN Ze-feng, et al. The initiation of local rolling contact fatigue on railway wheels: an experimental study[J]. International Journal of Fatigue, 2020, 132 (1): 105354. http://www.researchgate.net/publication/336861895_the_initiation_of_local_rolling_contact_fatigue_on_railway_wheels_an_experimental_study
    [26] DANIEL W J, PAL S, FARJOO M. Rail squats: progress in understanding the Australian experience[J]. Proceedings of the Institution of Mechanical Engineer, Part F: Journal of Rail and Rapid Transit, 2013, 227(5): 481-492. doi: 10.1177/0954409713500950
    [27] AI-JUBOORI A, ZHU H, WEXLER D. Characterisation of white etching layers formed on rails subjected to different traffic conditions[J]. Wear, 2019, 436/437(1): 202998. http://www.sciencedirect.com/science/article/pii/S0043164819301413
    [28] LI Zi-li, ZHAO Xin, ESVELD C, et al. An investigation into the causes of squats: correlation analysis and numerical modeling[J]. Wear, 2008, 265(9/10): 1349-55. http://www.sciencedirect.com/science/article/pii/S0043164808001567
    [29] 习年生, 刘丰收, 周清跃. 钢轨滚动接触疲劳缺陷的特征与发展模式[J]. 理化检验—物理分册, 2005, 41(增): 95-99.

    XI Nian-sheng, LIU Feng-shou, ZHOU Qing-yue. Characteristics and development modes of rail rolling contact fatigue[J]. Physical Testing and Chemical Analysis—Physical Testing, 2005, 41(S): 95-99.
    [30] 陈水友, 刘吉华, 郭俊, 等. 车轮材料特性对轮轨磨损与疲劳性能影响的研究[J]. 摩擦学学报, 2015, 35(5): 531-537. https://www.cnki.com.cn/Article/CJFDTOTAL-MCXX201505003.htm

    CHEN Shui-you, LIU Ji-hua, GUO Jun, et al. Effect of wheel material characteristics on wear and fatigue property of wheel-rail[J]. Tribology, 2015, 35(5): 531-537. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-MCXX201505003.htm
    [31] DONZELLA G, MAZZ A, PETROGALLI C. Competition between wear and rolling contact fatigue at the wheel-rail interface: some experimental evidence of rail steel[J]. Proceedings of the Institution of Mechanical Engineer, Part F: Journal of Rail and Rapid Transit, 2009, 223(1): 31-44. doi: 10.1243/09544097JRRT161
    [32] EADIE D T, ELVIDGE D, OLDKNOW K, et al. The effects of top of rail friction modifier on wear and rolling contact fatigue: full-scale rail-wheel test rig evaluation, analysis and modeling[J]. Wear, 2008, 265(9/10): 1222-1230. http://www.sciencedirect.com/science/article/pii/S0043164808001695
    [33] OLOFSSON U, NILSSON R. Surface cracks and wear of rail: a full-scale test on commuter train track[J]. Proceedings of the Institution of Mechanical Engineer, Part F: Journal of Rail and Rapid Transit, 2002, 216(4): 249-264. doi: 10.1243/095440902321029208
    [34] BOYACIOGLU P, BEVAN A, VICKERSTAFF A. Prediction of RCF damage on underground metro lines[C]//ZHAI Wan-ming. Proceedings of the 1st International Conference on Rail Transportation. Chengdu: Southwest Jiaotong University, 2017: 207-225.
    [35] FRANKLIN F J, WIDIYARTA I, KAPOOR A. Computer simulation of wear and rolling contact fatigue[J]. Wear, 2001, 251 (1/2): 949-955. http://www.sciencedirect.com/science/article/pii/S0043164801007323
    [36] FRANKLIN F J, GARNHAM J E, FLETCHER D I, et al. Modelling rail steel microstructure and its effect on crack initiation[J]. Wear, 2008, 265(9): 1332-1341. http://www.sciencedirect.com/science/article/pii/S0043164808001981
    [37] VASIC G, FRANKLIN F J. Modelling of plastic deformation and crack initiation in premium pearlitic rail steels[C]//GRASSIE K L, ZHANG Wei-hua. Proceedings of the 9th International Conference on Contact Mechanics and Wear of Rail/Wheel Systems. Chengdu: Southwest Jiaotong University, 2012: 372-378.
    [38] 丁军君, 孙树磊, 李芾, 等. 车轮滚动接触疲劳与磨耗耦合关系数值模拟[J]. 机械工程学报, 2012, 48(16): 86-90. https://www.cnki.com.cn/Article/CJFDTOTAL-JXXB201216016.htm

    DING Jun-jun, SUN Shu-lei, LI Fu, et al. Simulation of coupling relationship between wheel rolling contact fatigue and wear[J]. Journal of Mechanical Engineering, 2012, 48(16): 86-90. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-JXXB201216016.htm
    [39] WANG Shuai-shuai, ZHAO Xiu-juan, LIU Peng-tao, et al. Investigation of the relation between rolling contact fatigue property and microstructure on the surface layer of D2 wheel steel[J]. Materials Sciences and Applications, 2019, 10(8): 509-526. doi: 10.4236/msa.2019.108037
    [40] VARVANI-FARAHANI A, TOPPER T H. Crack growth and closure mechanisms of shear cracks under constant amplitude biaxial straining and periodic compressive overstraining in 1045 steel[J]. International journal of fatigue, 1997, 19(7): 589-596. doi: 10.1016/S0142-1123(97)00077-7
    [41] CLAYTON P. Tribological aspects of wheel-rail contact: a review of recent experimental research[J]. Wear, 1996, 191(1): 170-183. http://www.sciencedirect.com/science/article/pii/0043164895066519
    [42] JOHNSON K L. The strength of surfaces in rolling contact[J]. Proceedings of the Institution of Mechanical Engineers, Part C: Journal of Mechanical Engineering Science, 1989, 203(3): 151-163.
    [43] CHEN H, FUKAGAI S, SONE Y, et al. Assessment of lubricant applied to wheel/rail interface in curves[J]. Wear, 2014, 314(1/2): 228-35. http://www.sciencedirect.com/science/article/pii/S0043164813006029
    [44] TYFOUR W R, BEYNON J H, KAPOOR A. Deterioration of rolling contact fatigue life of pearlitic rail steel due to dry-wet rolling-sliding line contact[J]. Wear, 1996, 197(1): 255-265. http://www.sciencedirect.com/science/article/pii/0043164896069785
    [45] STEENBERGEN M. Squat formation and rolling contact fatigue in curved rail track[J]. Engineering Fracture Mechanics, 2015, 143(7): 80-96. http://www.sciencedirect.com/science/article/pii/S0013794415002945
    [46] BOWER A F. The influence of crack face friction and trapped fluid on surface initiated rolling contact fatigue cracks[J]. Journal of Tribology, 1988, 110(4): 704-711. doi: 10.1115/1.3261717
    [47] BOGDANSKI S, OLZAK M, STUPNICKI J. Numerical modelling of a 3D rail RCF squat-type crack under operating load[J]. Fatigue and Fracture of Engineering Materials and Structures, 1998, 21(8): 923-935. doi: 10.1046/j.1460-2695.1998.00082.x
    [48] CLAYTON P, HILL D N. Rolling contact fatigue of a rail steel[J]. Wear, 1987, 117(3): 319-334. doi: 10.1016/0043-1648(87)90152-9
    [49] FLETCHER D I, BEYNON J H. The effect of intermittent lubrication on the fatigue life of pearlitic rail steel in rolling-sliding contact[J]. Proceedings of the Institution of Mechanical Engineer, Part F: Journal of Rail and Rapid Transit, 2000, 214(3): 145-158. doi: 10.1243/0954409001531270
    [50] ISHIDA M, ABE N. Experimental study on rolling contact fatigue from the aspect of residual stress[J]. Wear, 1996, 191(1): 65-71. http://www.sciencedirect.com/science/article/pii/0043164895067124
    [51] SATO M, ANDERSON P M, RIGNEY D A. Rolling-sliding behavior of rail steels[J]. Wear, 1993, 162-164(4): 159-72. http://www.sciencedirect.com/science/article/pii/004316489390497A
    [52] LITTMANN W E, WIDNER R L, WOLFE J O, et al. The role of lubrication in propagation of contact fatigue cracks[J]. Journal of Tribology, 1968, 90(1): 89-100. http://www.researchgate.net/publication/273931759_Closure_to_Discussions_of_'The_Role_of_Lubrication_in_Propagation_of_Contact_Fatigue_Cracks'_1968_ASME_J_Lubr_Technol_90_p_630-632
    [53] KONDO K, YOROIZAKA K, SATO Y. Cause, increase, diagnosis, countermeasures and elimination of Shinkansen shelling[J]. Wear, 1996, 191(1): 199-203. http://www.sciencedirect.com/science/article/pii/0043164895067272
    [54] KALOUSEK J, MAGEL E, STRASSER J, et al. Tribological interrelationship of seasonal fluctuations of freight car wheel wear, contact fatigue shelling and composition brakeshoe consumption[J]. Wear, 1996, 191(1): 210-218. http://www.sciencedirect.com/science/article/pii/0043164895067000
    [55] FLETCHER D I, HYDE P, KAPOOR A. Modelling and full-scale trials to investigate fluid pressurisation of rolling contact fatigue cracks[J]. Wear, 2008, 265(9): 1317-1324. http://www.sciencedirect.com/science/article/pii/S0043164808001543
    [56] NIA S H, CASANUEVA C, STICHEL S. Prediction of RCF and wear evolution of iron-ore locomotive wheels[J]. Wear, 2015, 338/339(1): 62-72. http://www.sciencedirect.com/science/article/pii/S0043164815003300
    [57] HARDWICK C, LEWIS R, STOCK R. The effects of friction management materials on rail with pre-existing RCF surface damage[J]. Wear, 2017, 384/385(1): 50-60. http://www.sciencedirect.com/science/article/pii/S0043164816306111
    [58] EKBERG A, AKESSON B, KABO E. Wheel/rail rolling contact fatigue-probe, predict, prevent[J]. Wear, 2014, 314(1/2): 2-12. http://www.sciencedirect.com/science/article/pii/S0043164813006005
    [59] ARIAS-CUEVAS O, LI Zi-li, LEWIS R, Investigating the lubricity and electrical insulation caused by sanding in dry wheel-rail contact[J]. Tribology Letter, 2010, 37(3): 623-635. doi: 10.1007/s11249-009-9560-1
    [60] ZHAO Xin, WEN Ze-feng, ZHU Min-hao, et al. A study on high-speed rolling contact between a wheel and a contaminated rail[J]. Vehicle System Dynamics, 2014, 52(10): 1270-1287. doi: 10.1080/00423114.2014.934845
    [61] 张振先, 谭江, 黄双超, 等. 复杂运行环境下高速轮轨最佳撒砂增黏策略试验[J]. 中国铁道科学, 2020, 41(2): 123-130. doi: 10.3969/j.issn.1001-4632.2020.02.15

    ZHANG Zhen-xian, TAN Jiang, HUANG Shuang-chao, et al. Experimental study on optimum sanding and adhesion enhancement strategy for high speed wheel and rail under complicated operation environments[J]. China Railway Science, 2020, 41(2): 123-130. (in Chinese) doi: 10.3969/j.issn.1001-4632.2020.02.15
    [62] 张军, 王雪萍, 马贺. 第三介质对轮轨最大静摩擦因数影响的试验[J]. 机械工程学报, 2018, 54(18): 123-128. https://www.cnki.com.cn/Article/CJFDTOTAL-JXXB201818016.htm

    ZHANG Jun, WANG Xue-ping, MA He. Experimental study on the influence of the third medium on the wheel/rail maximum static friction coefficient[J]. Journal of Mechanical Engineering, 2018, 54(18): 123-128. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-JXXB201818016.htm
    [63] CAO X, HUANG W L, HE C G, et al. The effect of alumina particle on improving adhesion and wear damage of wheel/rail under wet conditions[J]. Wear, 2016, 348/349: 98-115. doi: 10.1016/j.wear.2015.12.004
    [64] FACCOLI M, PETROGALLI C, LANCINI M, et al. Effect of desert sand on wear and rolling contact fatigue behaviour of various railway wheel steels, Wear, 2017, 396/397: 146-161. http://www.sciencedirect.com/science/article/pii/S0043164817304064
    [65] LEWIS R, DWYER-JOYCE R S, Wheel-rail wear and surface damage caused by adhesion sanding[J]. Tribology Series, 2003, 43(1): 731-741. http://www.sciencedirect.com/science/article/pii/S0167892203801013
    [66] LIU Yong-feng, JIANG Tao, ZHAO Xin, et al. On the wheel rolling contact fatigue of high power ac locomotives running in complicated environments[J]. Wear, 2019, 436/437: 202956. doi: 10.1016/j.wear.2019.202956
    [67] 刘丰收. 高速铁路钢轨磨耗的跟踪研究[J]. 铁道建筑, 2016, 56(11): 120-123. https://www.cnki.com.cn/Article/CJFDTOTAL-TDJZ201611032.htm

    LIU Feng-shou. Tracing research on rail wear in high-speed railway[J]. Railway Engineering, 2016, 56(11): 120-123. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-TDJZ201611032.htm
    [68] TG/GL 127—2013, 铁路动车组运用维修规程[S].

    TG/GL 127—2013, railway EMU operation and maintenance regulations[S].
    [69] 中国国家铁路集团有限公司. 2019年全路钢轨伤损分析报告[R]. 北京: 中国国家铁路集团有限公司, 2020.

    China Railway. Report of rail failure on Chinese railway network[R]. Beijing: China Railway, 2020.
    [70] PLETZ M, DAVES W, YAO Wei-ping, et al. Multi-scale finite element modeling to describe rolling contact fatigue in a wheel-rail test rig[J]. Tribology International, 2014, 80(1): 147-155. http://www.sciencedirect.com/science/article/pii/S0301679X14002643
    [71] ZHAO Xin, ZHAO Xiao-gang, LIU Chao, et al. A study on dynamic stress intensity factors of rail cracks at high speeds by a 3D explicit finite element model of rolling contact[J]. Wear, 2016, 366/367(1): 60-70. http://www.sciencedirect.com/science/article/pii/S0043164816301156
    [72] GARNHAM J E, DAVIS C L. The role of deformed rail microstructure on rolling contact fatigue initiation[J]. Wear, 2008, 265(9/10): 1363-1372. http://www.sciencedirect.com/science/article/pii/S004316480800183X
    [73] JOHNSON K L. Contact mechanics[D]. London: Cambridge University Press, 1985.
    [74] HIRAKAWA K. Truth of derailment at Hatfield in UK[M]. Kyoto: Keibunsha, 2008. (in Japanese)
    [75] MAKINO T, KATO T, HIRAKAWA K. The effect of slip ratio on the rolling contact fatigue property of railway wheel steel[J]. International Journal of Fatigue, 2012, 36(1): 68-79. doi: 10.1016/j.ijfatigue.2011.08.014
    [76] EKBERG A, KABO E, ANDERSSON H. An engineering model for prediction of RCF of railway wheels[J]. Fatigue and Fracture of Engineering Materials and Structures, 2002, 25(10): 899-909. doi: 10.1046/j.1460-2695.2002.00535.x
    [77] DIRKS B, ENBLOM R. Prediction model for wheel profile wear and rolling contact fatigue[J] Wear, 2011, 271(1): 210-217.
    [78] KABO E, EKBERG A, TORSTENSSON P T, at al. Rolling contact fatigue prediction for rails and comparisons with test rig results[J]. Proceedings of the Institution of Mechanical Engineer, Part F: Journal of Rail and Rapid Transit, 2010, 224(4): 303-317. doi: 10.1243/09544097JRRT343
    [79] BURSTOW M C. Whole life rail model application and development for RSSB, continued development of an RCF damage parameter[R]. London: Rail Standards and Safety Board, 2004.
    [80] TUNNA J, SINCLAIR J, PEREZ J. The development of a wheel wear and rolling contact fatigue model[R]. London: Rail Standards and Safety Board, 2007.
    [81] BURSTOW M. Experience of premium grade rail steels to resist rolling contact fatigue RCF on GB network[J]. Ironmaking and Steelmaking, 2013, 40(2): 103-107. doi: 10.1179/1743281212Y.0000000042
    [82] HIENSCH M, STEENBERGEN M. Rolling contact fatigue on premium rail grades: damage function development from field data[J]. Wear, 2018, 394/395(1): 187-194. http://www.sciencedirect.com/science/article/pii/S0043164817313492
    [83] HILL D N, CLAYTON P. The development of a laboratory rolling contact fatigue testing procedure[R]. Derby: TMMF, 1982.
    [84] 刘颍宾, 宫彦华, 王强, 等. 列车车轮滚动接触疲劳裂纹评价研究[J]. 摩擦学学报, 2020, 40(3): 305-313. https://www.cnki.com.cn/Article/CJFDTOTAL-MCXX202003005.htm

    LIU Ying-bin, GONG Yan-hua, WANG Qiang, et al. Evaluation of rolling contact fatigue crack of train wheels[J]. Tribology, 2020, 40(3): 305-313. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-MCXX202003005.htm
    [85] RINGSBERG J W, LOO-MORREY M, JOSEFSON B L, et al. Prediction of fatigue crack initiation for rolling contact fatigue[J]. International Journal of Fatigue, 2000, 22(3): 205-215. doi: 10.1016/S0142-1123(99)00125-5
    [86] JIANG Yan-yao, SEHITOGLU H. A model for rolling contact failure[J]. Wear, 1999, 224(1): 38-49. doi: 10.1016/S0043-1648(98)00311-1
    [87] SANDSTRÖM J, EKBERG A. Numerical study of the mechanical deterioration of insulated rail joints[J]. Proceedings of the Institution of Mechanical Engineer, Part F: Journal of Rail and Rapid Transit, 2009, 223(3): 265-273. doi: 10.1243/09544097JRRT243
    [88] TALLIAN T E. Simplified contact fatigue life prediction model: part I. Review of published models, part Ⅱ. New model[J]. Journal of Tribology, 1992, 114(2): 207-220. doi: 10.1115/1.2920875
    [89] VAN K D, MAITOURNAM M H. On some recent trends in modeling of contact fatigue and wear in rail[J]. Wear, 2002, 253(1/2): 219-227. http://www.sciencedirect.com/science/article/pii/S0043164802001047
    [90] SAKALO V, SAKALO A, RODILOV A, et al. Computer modeling of processes of wear and accumulation of rolling contact fatigue damage in railway wheels using combined criterion[J]. Wear, 2019, 432/433(1): 102900.
    [91] LU C, NIETO J, PUY I, et al. Fatigue prediction of rail welded joints[J]. International Journal of Fatigue, 2018, 113(1): 78-87. http://www.sciencedirect.com/science/article/pii/S0142112318301300
    [92] LI Zi-li, ZHAO Xin, DOLLEVOET R. An approach to determine a critical size for rolling contact fatigue initiating from rail surface defects[J]. International Journal of Rail Transportation, 2017, 5(1): 16-37. doi: 10.1080/23248378.2016.1194775
    [93] 王延朋, 丁昊昊, 邹强, 等, 列车车轮踏面滚动接触疲劳研究进展[J]. 表面技术, 2020, 49(5): 120-128. https://www.cnki.com.cn/Article/CJFDTOTAL-BMJS202005016.htm

    WANG Yan-peng, DING Hao-hao, ZOU Qiang, et al. Research progress on rolling contact fatigue of railway wheel treads[J]. Surface Technology, 2020, 49(5): 120-128. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-BMJS202005016.htm
    [94] 肖乾, 方骏. 铁道车辆轮轨滚动接触疲劳裂纹研究综述[J]. 华东交通大学学报, 2015, 32(1): 16-21. doi: 10.3969/j.issn.1005-0523.2015.01.003

    XIAO Qian, FANG Jun. Research review on wheel-rail rolling contact fatigue crack of railway vehicles[J]. Journal of East China Jiaotong University, 2015, 32(1): 16-21. (in Chinese) doi: 10.3969/j.issn.1005-0523.2015.01.003
    [95] ZHAO Xin, LI Zi-li, DOLLEVOET R. The vertical and the longitudinal dynamic responses of the vehicle-track system to squat type short wavelength irregularity[J]. Vehicle System Dynamics, 2013, 51(12): 1918-1937. doi: 10.1080/00423114.2013.847466
    [96] ZHAO Xin, WEN Ze-feng, WANG Heng-yu, et al. Modeling of high-speed wheel-rail rolling contact on a corrugated rail and corrugation development[J]. Journal of Zhejiang University—Science A (Applied Physics and Engineering), 2014, 15(12): 946-963. doi: 10.1631/jzus.A1400191/figures/18
    [97] 寇峻瑜, 赵鑫, 张鹏, 等. 高速滚滑下轮轨表层材料的应变率水平估计[J]. 工程力学, 2019, 36(4): 239-247. https://www.cnki.com.cn/Article/CJFDTOTAL-GCLX201904027.htm

    KOU Jun-yu, ZHAO Xin, ZHANG Peng. Estimation of strain rates for wheel-rail surface materials under high-speed rolling-sliding contact[J]. Engineering Mechanics, 2019, 36(4): 239-247. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-GCLX201904027.htm
    [98] STOCK R, PIPPAN R. RCF and wear in theory and practice—the influence of rail grade on wear and RCF[J]. Wear, 2011, 271(1): 125-133. http://www.sciencedirect.com/science/article/pii/S0043164810003492
    [99] 王文健. 轮轨滚动接触疲劳与磨损耦合关系及预防措施研究[D]. 成都: 西南交通大学, 2008.

    WANG Wen-jian. Study on coupling relationship between rolling contact fatigue and wear of wheel-rail and prevention measures[D]. Chengdu: Southwest Jiaotong University, 2008. (in Chinese)
    [100] POINTNER P. High strength rail steels—the importance of material properties in contact mechanics problems[J]. Wear, 2008, 265 (9/10): 1373-1379. http://www.sciencedirect.com/science/article/pii/S0043164808001841
    [101] STEELE R K, REIFF R P. Rail: its behaviour and relationship to total system wear[C]//Federal Railroad Administration. Proceedings of International Heavy Haul Conference. Pueblo: Federal Railroad Administration, 1981: 115-164.
    [102] ZHAO Xin, LI Zi-li. The solution of frictional wheel-rail rolling contact with a 3-D transient finite element model: validation and error analysis[J]. Wear, 2011, 271(1/2): 444-452. http://www.sciencedirect.com/science/article/pii/S0043164810003418
    [103] ZHAO Xin, LI Zi-li. A three-dimensional finite element solution of frictional wheel-rail rolling contact in elasto-plasticity[J]. Journal of Engineering Tribology, 2015, 229(1): 86-100. doi: 10.1177/1350650114543717
    [104] ZHAO Xin, ZHANG Peng, WEN Ze-feng. On the coupling of the vertical, lateral and longitudinal wheel-rail interactions at high frequencies and the resulting irregular wear[J]. Wear, 2019, 430/431(1): 317-326. http://www.sciencedirect.com/science/article/pii/S0043164819300134
    [105] 周平宇, 马利军. 关于动车组车轮踏面浅表层损伤机理及对策[J]. 铁道车辆, 2015, 53(2): 30-31. doi: 10.3969/j.issn.1002-7602.2015.02.010

    ZHOU Ping-yu, MA Li-jun. The shallow surface damage mechanism of wheel treads for multiple units and counter measures[J]. Rolling Stock, 2015, 53(2): 30-31. (in Chinese) doi: 10.3969/j.issn.1002-7602.2015.02.010
    [106] 王培东, 郑静, 李富强. 动车组车轮踏面滚动接触疲劳安全评估研究[J]. 铁道车辆, 2020, 58(2): 12-13. https://www.cnki.com.cn/Article/CJFDTOTAL-TDCL202002005.htm

    WANG Pei-dong, ZHENG Jing, LI Fu-qiang. Studies into rolling contact fatigue of EMU wheels[J]. Rolling Stock, 2020, 58(2): 12-13. https://www.cnki.com.cn/Article/CJFDTOTAL-TDCL202002005.htm
    [107] CANTINI S, CERVELLO S. The competitive role of wear and RCF: full scale experimental assessment of artificial and natural defects in railway wheel treads[J]. Wear, 2016, 366/367(1): 325-37.
    [108] 张弘. 动车组车轮踏面浅表层裂纹成因分析[J]. 铁道机车车辆, 2006: 36(1): 6-9. doi: 10.3969/j.issn.1008-7842.2006.01.003

    ZHANG Hong. Reason analysis of shallow surface cracks on EMU wheels tread[J]. Railway Locomotive and Car, 2006, 36(1): 6-9. (in Chinese) doi: 10.3969/j.issn.1008-7842.2006.01.003
    [109] ZHAO Xiang-ji, GUO Jun, LIU Qi-yue, et al. Effects of spherical dents on microstructure evolution and rolling contact fatigue of wheel/rail materials[J]. Tribology International, 2018, 127(11): 520-532. http://www.sciencedirect.com/science/article/pii/S0301679X18303293
    [110] ZENG Dong-fang, XU Tian, LIU Wei-dong, et al. Investigation on rolling contact fatigue of railway wheel steel with surface defect[J]. Wear, 2020, 446/447(1): 203207. http://www.sciencedirect.com/science/article/pii/S0043164819314097
    [111] 蔡宇天, 赵鑫, 陈佳明, 等. 城际动车组车轮I类滚动接触疲劳机理研究[J]. 中南大学学报(自然科学版), 2020, 51(9): 2653-2662. https://www.cnki.com.cn/Article/CJFDTOTAL-ZNGD202009031.htm

    CAI Yu-tian, ZHAO Xin, CHEN Jiaming, et al. Study on initiation mechanism of rolling contact fatigue class I on intercity EMU wheels[J]. Journal of Central South University (Science and Technology), 2020, 51(9): 2653-2662. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-ZNGD202009031.htm
    [112] 王玉光, 卢纯, 赵鑫, 等. 高速动车组车轮滚动接触疲劳观测与模拟研究[J]. 机械工程学报, 2018, 54(4): 150-157. https://www.cnki.com.cn/Article/CJFDTOTAL-JXXB201804024.htm

    WANG Yu-guang, LU Cun, ZHAO Xin, et al. Rolling contact fatigue of Chinese high speed wheels: observations and simulations[J]. Journal of Mechanical Engineering, 2018, 54(4): 150-157. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-JXXB201804024.htm
    [113] MAGEL E, RONEY M, KALOUSEK J, et al. The blending of theory and practice in modern rail grinding[J]. Fatigue and Fracture of Engineering Materials and Structures, 2003, 26(1): 921-929. doi: 10.1046/j.1460-2695.2003.00669.x
    [114] CUI Da-bin, WANG Heng-yu, LI Li, et al. Optimal design of wheel profiles for high-speed trains[J]. Proceedings of the Institution of Mechanical Engineer, Part F: Journal of Rail and Rapid Transit, 2015, 229(3): 248-261. doi: 10.1177/0954409713509979
    [115] 王晓东, 林晓晨, 李培署. 和谐号CRH6型动车组制动减速度设计与控制[J]. 铁道车辆, 2016, 54(6): 15-19, 4. doi: 10.3969/j.issn.1002-7602.2016.06.005

    WANG Xiao-dong, LIN Xiao-chen, LI Pei-shu. Design and control of the braking deceleration of the CRH6 multiple units[J]. Rolling Stock, 2016, 54(6): 15-19, 4. (in Chinese) doi: 10.3969/j.issn.1002-7602.2016.06.005
    [116] 丁叁叁, 张忠敏, 何丹炉, 等. 城际动车组总体技术设计[J]. 机车电传动, 2014(6): 10-15. https://www.cnki.com.cn/Article/CJFDTOTAL-JCDC201406005.htm

    DING San-san, ZHANG Zhong-min, HE Dan-lu, et al. Overall technical design of intercity EMUs[J]. Electric Drive for Locomotives, 2014(6): 10-15. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-JCDC201406005.htm
    [117] 何成刚, 周桂源, 王娟, 等. 曲率半径对车轮滚动接触疲劳性能的影响[J]. 摩擦学学报, 2014, 34(3): 256-261. https://www.cnki.com.cn/Article/CJFDTOTAL-MCXX201403007.htm

    HE Cheng-gang, ZHOU Gui-yuan, WANG Juan, et al. Effect of curve radius of rail on rolling contact fatigue properties of wheel steel[J]. Tribology, 2014, 34(3): 256-261. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-MCXX201403007.htm
    [118] ZHOU Gui-yuan, HE Cheng-gang, WEN Guang, et al. Fatigue damage mechanism of railway wheels under lateral forces[J]. Tribology International, 2015, 91(1): 160-169. http://www.sciencedirect.com/science/article/pii/S0301679X15002935
    [119] 李霞, 温泽峰, 金学松. 重载铁路车轮磨耗与滚动接触疲劳研究[J]. 铁道学报, 2011, 33(3): 28-34. doi: 10.3969/j.issn.1001-8360.2011.03.005

    LI Xia, WEN Ze-feng, JIN Xue-song. Investigation into wheel wear and fatigue of heavy-haul railways[J]. Journal of the China Railway Society, 2011, 33(3): 28-34. (in Chinese) doi: 10.3969/j.issn.1001-8360.2011.03.005
    [120] HUANG Y B, SHI L B, ZHAO X J, et al. On the formation and damage mechanism of rolling contact fatigue surface cracks of wheel/rail under the dry condition[J]. Wear, 2018, 400/401(1): 62-73.
    [121] 邓建辉, 刘启跃, 王飞龙, 等. 车速对钢轨接触疲劳伤损的影响及高速线路钢轨选用[J]. 钢铁钒钛, 2006, 27(3): 48-54. doi: 10.3969/j.issn.1004-7638.2006.03.010

    DENG Jian-hui, LIU Qi-yue, WANG Fei-long, et al. Influence of train velocity on rail contact fatigue damage and how to select rail for high-speed[J]. Iron Steel Vanadium Titanium, 2006, 27(3): 48-54. (in Chinese) doi: 10.3969/j.issn.1004-7638.2006.03.010
    [122] XIAO Qian, ZHENG Ji-feng, LIU Ji-hua, et al. Analysis of the wheel/rail rolling contact fatigue of a high-speed train under the transient mechanism[J]. Journal of Mechanical Science and Technology, 2017, 31(5): 2235-2242. doi: 10.1007/s12206-017-0420-x
    [123] NIELSEN J C O, EKBERG A. Acceptance criterion for rail roughness level spectrum based on assessment of rolling contact fatigue and rolling noise[J]. Wear, 2011, 271(1/2): 319-327. http://www.sciencedirect.com/science/article/pii/S0043164810003479
    [124] EKBERG A, KABO E, NIELSEN J C O, et al. Subsurface initiated rolling contact fatigue of railway wheels as generated by rail corrugation[J]. International Journal of Solids and Structures, 2007, 44(24): 7975-7987. doi: 10.1016/j.ijsolstr.2007.05.022
    [125] MA L, HE C G, ZHAO X J, et al. Study on wear and rolling contact fatigue behaviors of wheel/rail materials under different slip ratio conditions[J]. Wear, 2016, 366/367(1): 13-26.
    [126] 张聪聪, 周宇, 黄旭炜, 等. 高速铁路钢轨预打磨策略及伤损发展特征[J]. 华东交通大学学报, 2019, 36(2): 33-40. https://www.cnki.com.cn/Article/CJFDTOTAL-HDJT201902006.htm

    ZHANG Cong-cong, ZHOU Yu, HUANG Xun-wei, et al. Research on the rail pre-grinding strategy and growth characteristics of rail defects in high-speed railway[J]. Journal of East China Jiaotong University, 2019, 36(2): 33-40. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-HDJT201902006.htm
    [127] STONE D H. Rolling contact fatigue origins of wheel failures in heavy haul service[C]//GRASSIE K L, ZHANG Wei-hua. Proceedings of 9th International Conference on Contact Mechanics and Wear of Rail/Wheel Systems. Chengdu: Southwest Jiaotong University, 2012, 19-27.
    [128] 王家玉, 王顺福. 机车轮对JM、JM2、JM3磨耗型踏面及其剥离[J]. 内燃机车, 2009(5): 34-37. doi: 10.3969/j.issn.1003-1820.2009.05.011

    WANG Jia-yu, WANG Shun-fu. Worn profile tread JM, JM2 and JM3 for locomotive wheel and the tread shelled-out[J]. Diesel Locomotives, 2009(5): 34-37. (in Chinese) doi: 10.3969/j.issn.1003-1820.2009.05.011
    [129] LIU Yong-feng, JIANG Tao, ZHAO Xin, et al. Effects of axle load transfer on wheel rolling contact fatigue of high-power AC locomotives with oblique traction rods[J]. International Journal of Fatigue, 2020, 139(1): 105748. http://www.sciencedirect.com/science/article/pii/S0142112320302796
    [130] LYU Kai-kai, WANG Kai-yun, LIU Peng-fei, et al. Analysis on the features and potential causes of wheel surface damage for heavy-haul locomotives[J]. Engineering Failure Analysis, 2019, 109(1): 104292. http://www.sciencedirect.com/science/article/pii/S135063071930785X
    [131] 吕凯凯. 大功率电力机车踏面剥离产生机制的理论与试验研究[D]. 成都: 西南交通大学, 2020.

    LYU Kai-kai. Theoretical and experimental investigation into the generation mechanism of wheel tread spalling on high-power electric locomotive[D]. Chengdu: Southwest Jiaotong University, 2020. (in Chinese)
    [132] 王文斌. HXD2C型机车轮对踏面剥离问题的分析研究[J]. 机车电传动, 2017(4): 113-116. https://www.cnki.com.cn/Article/CJFDTOTAL-JCDC201704031.htm

    WANG Wen-bin. A study on wheel spalling of HXD2C locomotives[J] Electric Drive for Locomotives, 2017(4): 113-116. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-JCDC201704031.htm
    [133] 崔银会, 张斌. 200 km·h-1轻型客车车轮踏面剥离原因分析[J]. 轧钢, 2003, 20(3): 13-15. doi: 10.3969/j.issn.1003-9996.2003.03.005

    CUI Yin-hui, ZHANG Bin. Analysis of the shelling causes of wheel tread of 200 km·h-1 light passenger train[J]. Steel Rolling, 2003, 20(3): 13-15. (in Chinese) doi: 10.3969/j.issn.1003-9996.2003.03.005
    [134] 陶功权, 王衡禹, 赵鑫, 等. 基于轮轨关系的车轮踏面损伤机理研究[J]. 机械工程学报, 2013, 49(18): 23-29. https://www.cnki.com.cn/Article/CJFDTOTAL-JXXB201318004.htm

    TAO Gong-quan, WANG Heng-yu, ZHAO Xin, et al. Research on wheel tread damage mechanism based on interaction of wheel and rail[J]. Journal of Mechanical Engineering, 2013, 49(18): 23-29. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-JXXB201318004.htm
    [135] 陶功权. KKD客车车轮踏面剥离成因初探[D]. 成都: 西南交通大学, 2013.

    TAO Gong-quan. Preliminary study on the cause of wheel tread shelling of KKD passenger car[D]. Chengdu: Southwest Jiaotong University, 2013. (in Chinese)
    [136] ZHOU Yu, WANG Shao-feng, WANG Tian-yi, et al. Field and laboratory investigation of the relationship between railhead check and wear in a heavy-haul railway[J]. Wear, 2014, 315(1/2): 68-77. http://www.sciencedirect.com/science/article/pii/S0043164814001264
    [137] 周宇, 张杰, 杨新文, 等. U75V热处理钢轨滚动接触疲劳裂纹和磨耗试验[J]. 同济大学学报(自然科学版), 2015, 43(6): 877-881. https://www.cnki.com.cn/Article/CJFDTOTAL-TJDZ201506011.htm

    ZHOU Yu, ZHANG Jie, YANG Xin-wen, et al. Experiment on the rolling contact fatigue crack and wear of U75V heat-treated rail[J]. Journal of Tongji University (Natural Science), 2015, 43(6): 877-881. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-TJDZ201506011.htm
    [138] 周宇, 李骏鹏, 司道林. 普速铁路钢轨滚动接触疲劳裂纹萌生研究和检验[J]. 铁道建筑, 2020, 60(5): 107-111. doi: 10.3969/j.issn.1003-1995.2020.05.25

    ZHOU Yu, LI Jun-peng, SI Dao-lin. Research and validation on rolling contact fatigue crack initiation in existing common speed railway[J]. Railway Engineering, 2020, 60(5): 107-111. (in Chinese) doi: 10.3969/j.issn.1003-1995.2020.05.25
    [139] 刘学文, 邹定强, 邢丽贤, 等. 钢轨踏面斜裂纹伤损原因及对策的研究[J]. 中国铁道科学, 2004, 25(2): 82-87. doi: 10.3321/j.issn:1001-4632.2004.02.017

    LIU Xue-wen, ZOU Ding-qiang, XING Li-xian. Causes of tread oblique crack and countermeasures[J]. China Railway Science, 2004, 25(2): 82-87. (in Chinese) doi: 10.3321/j.issn:1001-4632.2004.02.017
    [140] 赵雪芹, 王文健, 郭俊, 等. 广深线PD3与U71Mn钢轨斜裂纹形成特性分析[J]. 润滑与密封, 2007, 32(3): 35-37. doi: 10.3969/j.issn.0254-0150.2007.03.011

    ZHAO Xue-qin, WANG Wen-jian, GUO Jun, et al. An investigation on formation characteristic of oblique crack of PD3 and U71Mn rail in Guangzhou-Shenzhen Railway[J]. Lubrication Engineering, 2007, 32(3): 35-37. (in Chinese) doi: 10.3969/j.issn.0254-0150.2007.03.011
    [141] 钟雯. 钢轨的损伤机理研究[D]. 成都: 西南交通大学, 2011.

    ZHONG Wen. Experimental investigation of rail damnification mechanism[D]. Chengdu: Southwest Jiaotong University, 2011. (in Chinese)
    [142] 熊嘉阳. 钢轨斜裂纹形成机理研究[D]. 成都: 西南交通大学, 2006.

    XIONG Jia-yang. Study on the formative mechanism of rail oblique crack[D]. Chengdu: Southwest Jiaotong University, 2006. (in Chinese)
    [143] 郭俊. 轮轨滚动接触疲劳损伤机理研究[D]. 成都: 西南交通大学, 2006.

    GUO Jun. Study on mechanism of wheel-rail rolling contact fatigue and damage[D]. Chengdu: Southwest Jiaotong University, 2006. (in Chinese)
    [144] 周宇, 黄旭炜, 王树国, 等. 考虑轨道几何不平顺的钢轨裂纹萌生与磨耗共存预测[J]. 同济大学学报(自然科学版), 2019, 47(11): 1600-1608. doi: 10.11908/j.issn.0253-374x.2019.11.009

    ZHOU Yu, HUANG Xun-wei, WANG Shu-guo, et al. Prediction of rail rolling contact fatigue crack initiation and wear growth considering track geometry irregularity[J]. Journal of Tongji University(Natural Science), 2019, 47(11): 1600-1608. (in Chinese) doi: 10.11908/j.issn.0253-374x.2019.11.009
    [145] 叶都玮. 城市轨道交通车辆车轮踏面缺陷产生的机理和预防措施[J]. 城市轨道交通研究, 2011, 14(1): 106-109. doi: 10.3969/j.issn.1007-869X.2011.01.025

    YE Du-wei. Mechanism of urban mass transits wheel tread defects and preventive measures[J]. Urban Mass Transit, 2011, 14(1): 106-109. (in Chinese) doi: 10.3969/j.issn.1007-869X.2011.01.025
    [146] 陈佳明, 赵鑫, 蔡宇天, 等. 地铁车轮轮缘根部滚动接触疲劳机理研究[J]. 铁道科学与工程学报, 2020, 17(9): 2372-2380. https://www.cnki.com.cn/Article/CJFDTOTAL-CSTD202009024.htm

    CHEN Jia-ming, ZHAO Xin, CAI Yu-tian, et al. Investigation on rolling contact fatigue mechanism of metro wheel flange root[J]. Journal of Railway Science and Engineering, 2020, 17(9): 2372-2380. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-CSTD202009024.htm
    [147] 温邦. 地铁车轮踏面滚动接触疲劳形成机理及对策研究[D]. 成都: 西南交通大学, 2017.

    WEN Bang. Study on mechanism and countermeasure of rolling contact fatigue of metro tread[D]. Chengdu: Southwest Jiaotong University, 2017. (in Chinese)
    [148] 梁喜仁, 陶功权, 陆文教, 等. 地铁钢轨滚动接触疲劳损伤研究[J]. 机械工程学报, 2019, 55(2): 147-155. https://www.cnki.com.cn/Article/CJFDTOTAL-JXXB201902017.htm

    LIANG Xi-ren, TAO Gong-quan, LU Wen-jiao, et al. Study on the rail rolling contact fatigue of subway[J]. Journal of Mechanical Engineering, 2019, 55(2): 147-155. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-JXXB201902017.htm
    [149] 张合吉, 何泽寒, 刘建桥, 等. 地铁异常磨耗车轮与辙叉接触分析[J]. 机械工程学报, 2018, 54(4): 117-123. https://www.cnki.com.cn/Article/CJFDTOTAL-JXXB201804019.htm

    ZHANG He-ji, HE Ze-han, LIU Jian-qiao, et al. Analysis of contact between frog and metro wheel tread with abnormal wear[J]. Journal of Mechanical Engineering, 2018, 54(4): 117-123. (in Chinese) https://www.cnki.com.cn/Article/CJFDTOTAL-JXXB201804019.htm
    [150] ZHAI Wan-ming, JIN Xue-song, WEN Zen-feng, et al. Wear problems of high-speed wheel/rail systems: observations, causes, and countermeasures in China[J]. Applied Mechanics Reviews, 2020, 72(1): 060801.
  • 加载中
图(42) / 表(1)
计量
  • 文章访问数:  3891
  • HTML全文浏览量:  1114
  • PDF下载量:  3351
  • 被引次数: 0
出版历程
  • 收稿日期:  2020-11-10
  • 刊出日期:  2021-08-27

目录

    /

    返回文章
    返回